The study found that a hybrid reinforcement of 0.5 wt% nylon fiber and 0.5 wt% glass fiber with 1.0 wt% of styrene butadiene rubber (SBR) mixed PMMA denture base material showed the highest impact, flexural, and compressive strength, which were about 84%, 58%, and 67% higher than the pure PMMA (control group), respectively.